Yb掺杂原子数分数为0.5%的Yb∶Y_3Al_5O_(12)晶体的光谱分析 被引量:9

Spectroscopic Properties of Yb∶Y_3Al_5O_(12) with Yb-DopingConcentration 0.5 at.-%
原文传递
导出
摘要 采用提拉法生长了Yb掺杂原子数分数为0.5%的Yb∶Y3Al5O12(Yb∶YAG)晶体,对晶体的吸收光谱和荧光光谱进行了分析。与Yb掺杂原子数分数为5%的Yb∶YAG晶体进行了对比,得出采用940 nm激光二极管(LD)抽运晶体最为合适。原子数分数为0.5%的Yb∶YAG晶体相对于原子数分数为5%的Yb∶YAG晶体自吸收效应的影响要小。测量了原子数分数为0.5%的Yb∶YAG晶体的荧光寿命为0.95 ms,与理论值很接近。因此采用原子数分数为0.5%的Yb∶YAG晶体作为激光工作物质将有利于高效、小型集成化的固体激光器的发展。 Yb:Y3Al5O12(Yb:YAG) single crystal with Yb doping concentration 0.5 at.-% was grown by the Czochralski process. The absorption spectra and fluorescence spectra were studied and compared with 5 at.-% Yb; YAG single crystal. All results indicate that as a laser cyrstal, 0. 5 at.-% Yb: YAG single crystal is suitable for pumping with 940 nm laser diode (LD) and the self-absorption effect is smaller than that of 5 at,-% Yb: YAG single crystal, The fluorescent lifetime of 0.5 at. -% Yb: YAG is 0.95 ms that is close to theoretical value. So this crystal is more promising as laser operation material used for high efficiency, miniature type, compact solid-state lasers.
出处 《中国激光》 EI CAS CSCD 北大核心 2006年第5期692-696,共5页 Chinese Journal of Lasers
基金 国家863计划(2002AA311030)资助项目
关键词 材料 光谱 YB:YAG晶体 吸收光谱 荧光光谱 自吸收 荧光寿命 materials spectrum Yb:YAG crystal absorption spectra fluorescence spectra self absorption fluorescent lifetime
  • 相关文献

参考文献4

二级参考文献26

共引文献109

同被引文献93

引证文献9

二级引证文献47

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部