摘要 针对矿渣、粉煤灰的成分及特点,研制了一种无熟料矿渣粉煤灰胶凝材料,并对其强度影响因素、水化性能进行了研究。结果表明,加入70%矿渣,15%粉煤灰,10%石膏,5%复合激发剂,可以制备性能较好的胶凝材料,28d抗压强度可达到58.21MPa。 According to composition and features of slag and fly ash,the cementitious material without clinker has been made and its strength influencing factors and the hydration capability have been studied. The results are as follows:the high-strength cementitious material can be made by adding 70 percent of slag, 15 percent of fly ash, 10 percent of gypsum and 5 percent of complex activated material and the compression strength at 28 d is up to 52.81 MPa.
出处 《新型建筑材料》 北大核心 2007年第12期8-11,共4页 New Building Materials
基金 国家科技支撑计划课题资助(2006BAC21B03)
关键词 矿渣 粉煤灰 复合激发剂 胶凝材料 slag fly ash complex activated material cementitious material
  • 相关文献

参考文献4

二级参考文献32

共引文献62

同被引文献81

引证文献8

二级引证文献29

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部