摘要 采用溶胶 -凝胶方法合成了锂二次电池阴极材料 Li( Cox Al1 - x) O2 ,并采用 XRD方法分析了材料的相变过程、烧结时间对材料合成的影响及不同 Al/Co比掺杂对材料相变的影响 ,并进行了结构表征 .研究表明 ,材料结构随 Al固溶度的增大及温度的升高呈现出 a轴缩短 ,c轴伸长的趋势 .材料晶相稳定温度在60 0~ 90 0℃之间 ,烧结时间在 3 The cathode material for lithium batteries Li(Co x Al 1-x )O 2 has been synthesized by sol gel technique. The effects of sintering temperature, sintering time and the molar ratio of Al and Co on the phase behavior of material was investigated via X ray diffraction. It is shown that the suitable synthetic and processing condition is that the sintering temperature is in the range of 600—900 ℃ and the sintering time is over 3 h.
出处 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 2000年第4期497-500,共4页 Chemical Journal of Chinese Universities
基金 国家自然科学基金 !(批准号 :197740 2 8)
关键词 锂电池 阴极材料 溶胶-凝胶 Li(CoxAl1-x)O2 Li battery Cathode material Sol gel method Synthesis X ray diffraction Phase behavior
  • 相关文献

参考文献15

二级参考文献161

共引文献1070

同被引文献62

  • 1周欣山,沈十林,倪瑞澄,熊樱菲.焙烧工艺对LiCoO_2结构和性能的影响[J].电池工业,2000,5(5):202-204. 被引量:3
  • 2王兴杰 等.柠檬酸溶胶凝胶法制备LiCoO2电极材料及其表征[J].无机化学,2004,20(5):608-608.
  • 3Nagaura T,Tozawa K.Prog.Batts.SOL[J].1990,9:209~217
  • 4Ohzuku T,Ueda A.J.Electrochem.Soc[J].1993,140:1862~1870
  • 5Rougier A,Gravereau p,Delmas C.J.Electrochem.Soc[J].1996,143:1168~1175
  • 6Aydionl M.K,Kohan A.F,Ceder G.Phys.Rev.B[J].1997,56:1354~1365.
  • 7Geder G,Chiang Y.M,Sadoway D.R Nature[J].1998,392:694~696.
  • 8Marezion M,Remeika J.P.J.Chem.Phys[J].1996,44:3143~3144.
  • 9Ferrare J.R,Nakamoto K.Introductory Raman Spectroscopy[M].Boston:Ademic Press,1994,Chapter1.
  • 10Inaba M,Iriyama Y,Ogumi Z.J.Raman Spectrosc[J].1997,28:613~617.

引证文献10

二级引证文献26

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部