以缓蚀剂钼酸盐插层水滑石(HT-MoO42-)为吸附剂,对NaCl溶液中的Cl-进行吸附,探讨了吸附时间、温度和Cl-初始浓度等因素对吸附的影响。测定了HT-MoO42-吸附Cl-前后的元素组成变化,测定了吸附等温线和吸附动力学曲线。结果表明,该吸附反应为介孔单分子层与多分子层吸附相结合,在70 h内达到吸附平衡,吸附量随Cl-初始浓度、温度的增加而增大,吸附过程遵循Lagergren二级反应动力学过程,相关系数R2为0.9981。
Corrosion inhibitor molybdate intercalated hydrotalcite as absorbent were used to adsorb CI- from NaC1 solu- tion. The effects of the adsorption time, adsorption temperature and initial concentration of the adsorbate ( CI- ) were investiga- ted. The element change of HT-MoO42- powers was admeasured before and after adsorption CI-, and adsorption isotherm and ad- sorption kinetic curve were determined. The experimental results showed that the adsorption reaction mainly proceeded in the form of Mesoporous monolayer combined with multilayer adsorption. The adsorption reached balance within 70h. The adsorption capacity was enhanced with the increase of initial chloride concentrations and temperature. The adsorption kinetics was followed Lagergren pseudo-second-order kinetic model with correlation coefficients of 0. 9981.
出处
《表面技术》
EI
CAS
CSCD
北大核心
2012年第6期26-29,共4页
Surface Technology
基金
广东省科技计划项目(2012B010500028)
广东石油化工学院自然科学基金(510009)
关键词
钼酸盐插层水滑石
Cl-
缓蚀剂
吸附动力学
molybdate intercalated hydrotalcite
chloride ion
corrosion inhibitor
adsorption kinetics