综述了碱溶胀法合成核壳中空微球的国内外研究进展,重点介绍了核壳中空结构的合成以及各种因素如聚合物组成,碱处理条件、乳化剂用量、单体瞬时转化率以及玻璃化温度对微球形态的影响。
The progress in preparation of hollow core-shell microspheresby alkali swelling method at home and abroad were reviewed and the synthesis of core-shell hollow structure and a variety of factors,such as polymer composition,alkali treatment condition,emulsifier amount,monomer instantaneous conversion rate and glass transition temperature on the morphology of the microspheres were emphatically introduced.