期刊文献+

利用非焦煤低碳炼铁新技术的初步研究 被引量:2

Investigation on a Novel Consideration of Ironmaking Process Using Non-Coking Coal
原文传递
导出
摘要 通过对非焦煤与铁矿粉"干馏"特征的试验调查分析,提出了"非炼焦煤与铁矿粉"共处理的低碳炼铁预处理技术路线。研究表明:干馏温度800℃,铁矿粉还原度可达到约78%,其中部分金属铁为氢元素所还原,可降低铁氧化物还原过程CO2排放量。 The low-carbon ironmaking technology on co-treatment of non-coking coal and iron-ore fines was proposed through investigating the characteristics of carbonization of non-coking coal and iron ore.The results showed that the percent metallization of the iron ore fines was up to 78% at 800 ℃ of carbonization temperature.Some metallic iron was already reduced by hydrogen,and the amount of CO2 release would be reduced.
出处 《中国冶金》 CAS 2012年第7期14-18,23,共6页 China Metallurgy
关键词 炼铁 非焦煤 氢还原 低碳 ironmaking non-coking coal hydrogen reduction low carbon
  • 相关文献

参考文献3

  • 1李维国.关于COREX一3000生产情况和需要攻关的技术问题[C]//2008年非高炉炼铁年会文集.延吉:中国金属学会,2008.
  • 2张青,郭丽.宝钢COREX-3000竖炉操作分析及改进[c]//2008年非高炉炼铁年会文集.延吉:中国金属学会,2008.
  • 3许海发,吴胜利,李肇毅,等.COREX一3000预还原竖炉的冶炼特点分析[c]//2008年非高炉炼铁年会文集.延吉:中国金属学会,2008.

同被引文献30

  • 1UJISAWA Y,NAKANO K,MATSUKU Y etc. Subjects for achievement of blast furnac operation with low reducing agentrate[J]. Tetsu-to-Hagane,2006,92(12):1015-1021.
  • 2Word Steel Association. World Steel in Figures 2009[R]. Brussels:Word Steel Association,2009:15.
  • 3HIRAKI K,YAMAZAKI Y,KANAI T etc. Numerical analysis of 3-D microstructure of coke using micro X-ray CT[J]. ISIJInternational,2012,52(11):1966-1972.
  • 4NOMURA S,H1GUCH1 K,KUNITOMO K etc. Reaction behavior of formed iron coke and its effect of decreasing thermalreserve zone temperature in blast furnace[J]. Tetsu-to-Hagan,2009,95(12):813-820.
  • 5NOMURA S,AYUKAWA H. Improvement in blast furnace reaction efficiency through the use of highly reactive calciumrich coke[J]. ISIJ International?2005,45(3):316-324.
  • 6SHARMA A,UEBO K?KUBOTA Y. Role of Fe203 and CaCOg on the development of carbon structure of coke and theircatalytic activity for gasification[J]. Tetsu-to-Hagan,2010,96(5):280-287.
  • 7KANNARI N,HARADA Y and FUJIMOTO H etc. Influence of Fe2O3 and CaCO3 addition on the coking of gooneylla coal[J]. Tetsu-to-Hagan,2010,96(5):249-257.
  • 8KONISHI H,USUI T,YAMASHITA A. Effect of residual volatile matter on reduction reaction between Semi-coal-char andiron oxide[J]. Tetsu-to-Hagan,2009,95(6):467-472.
  • 9Takashi A,Kiyoshi F,Hidekazu F. Development of carbon iron composite process[J]. JFE,2008,11(22):20-24.
  • 10NOMURA S,TERASHIMA H,SATO E,et al. Some fundamental aspects of highly reactive iron coke production [J].Tetsu-to-Hagan,2006,92(12):849-856.

引证文献2

二级引证文献5

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部