期刊文献+

Structural characterization of steam-heat treated Tectona grandis wood analyzed by FT-IR and 2D-IR correlation spectroscopy 被引量:4

Structural characterization of steam-heat treated Tectona grandis wood analyzed by FT-IR and 2D-IR correlation spectroscopy
原文传递
导出
摘要 The properties of wood can be improved through steam-heat treatment.There are many studies about mechanical properties of steam-heat treated wood,but very few studies are on the aspects of chemical modifications.In this study,FT-IR spectra combined with SD-IR spectra,correlation coefficients and 2DIR spectra are employed to analyze the chemical modifications of teak[Tectona grandis L.F.) wood during steam-heat treatment under treatment temperatures from 120 ℃ to 220 ℃ at intervals of 20 ℃.Acetic acid,which is produced during steam-heat treatment,acts as a catalyst of condensation and degradation reactions of wood components.The changes of wood components are more and more intense with increasing the treatment temperature.The sensitivity of wood samples to thermal perturbation rises initially with increasing treatment temperature before falling back.The steam-heat treated wood under180℃ is the most sensitive. The properties of wood can be improved through steam-heat treatment.There are many studies about mechanical properties of steam-heat treated wood,but very few studies are on the aspects of chemical modifications.In this study,FT-IR spectra combined with SD-IR spectra,correlation coefficients and 2DIR spectra are employed to analyze the chemical modifications of teak[Tectona grandis L.F.) wood during steam-heat treatment under treatment temperatures from 120 ℃ to 220 ℃ at intervals of 20 ℃.Acetic acid,which is produced during steam-heat treatment,acts as a catalyst of condensation and degradation reactions of wood components.The changes of wood components are more and more intense with increasing the treatment temperature.The sensitivity of wood samples to thermal perturbation rises initially with increasing treatment temperature before falling back.The steam-heat treated wood under180℃ is the most sensitive.
出处 《Chinese Chemical Letters》 SCIE CAS CSCD 2015年第2期221-225,共5页 中国化学快报(英文版)
基金 sponsored by the National Natural Science Foundation of China(No.31270591) Province-Academy Cooperation Project of Zhejiang Province and Chinese Academy of Forestry(No.2013SY01)
关键词 Teak wood Steam-heat treatment FT-IR spectroscopy The correlation coefficients 2D-IR spectroscopy Teak wood Steam-heat treatment FT-IR spectroscopy The correlation coefficients 2D-IR spectroscopy
  • 相关文献

参考文献2

二级参考文献11

  • 1C.W. Robertson, D. Williams, J. Opt. Soc. Am. 61 (1971) 1316.
  • 2LL. Tyler, G. Taylor, M.R. Querry, Appl. Opt. 17 (1978) 960.
  • 3D.M. Wieliczka, S.S. Weng, M.R. Querry, Appl. Opt. 28 (1989) 1714.
  • 4X.Q. Lin, K.M. Kadish, Proc. 2nd Conf. Exhib. Instrum. Anal., Beijing, (1987), p. 1311.
  • 5X.Q. Lin, Z.X. Zhang, W.Q. Hu, Chin. Chem. Lett. 22 (2011) 481.
  • 6A. Bewick, K. Kunimatsu, B.S. Pons, Electrochim. Acta 25 (1980) 465.
  • 7D.K. Roe, J.K. Sass, D.S. Bethune, et al. J. Electroanal. Chem. 216 (1987) 293.
  • 8A.1. Bo, X.Q. Lin, Chin. Chem. Lett. 9 (9) (1998) 851.
  • 9X.Q. Lin, Z.L. Li, Chin. Chem. Lett. 3 (1992) 1029.
  • 10X.Q. Lin, K.M. Kadish, Anal. Chem. 58 (1986) 1493.