摘要 During long-term use,the clay checker bricks for regenerators of coke ovens on gas side react with the impurities containing Fe and K20,causing foaming,softening and deformation,which is not only related with the impurity content and properties of the clay checker bricks,but also related with the type and the composition of the dust in the gas.After long term use,the clay checker bricks of coke ovens on air side have relative lower impurities containing Fe and K20.The inferior clay checker bricks,with high impurity content and high porosity,are easy to pulverize and deteriorate due to the oxidationreduction reaction with the iron oxide and the gas.The gas quality shall be concerned for long service life of the coke oven regenerators. During long-term use, the clay checker bricks for regenerators of coke ovens on gas side react with the impurities containing Fe and K2O, causing foaming, softening and deformation, which is not only related with the impurity content and properties of the clay checker bricks, but also related with the type and the composition of the dust in the gas. After long term use, the clay checker bricks of coke ovens on air side have relative lower impurities containing Fe and K2O. The inferior clay checker bricks, with high impurity content and high porosity, are easy to pulverize and deteriorate due to the oxidationreduction reaction with the iron oxide and the gas. The gas quality shall be concerned for long service life of the coke oven regenerators.
出处 《China's Refractories》 CAS 2019年第4期7-11,共5页 中国耐火材料(英文版)
关键词 coke oven REGENERATOR checker brick REFRACTORIES coke oven regenerator checker brick refractories
  • 相关文献

参考文献5

二级参考文献20

  • 1高振昕,卫晓辉,任钢伟,常亮,黄振武,刘卓峰.用后焦炉硅砖的显微结构[J].耐火材料,2005,39(2):140-145. 被引量:3
  • 2KonopicyK,LepereKE,RoutschkaG,etal.Untersuchungenangebrauchtensilikasteinenausdenkammerwaendenvonkoksofenbatterien[J].Tonind-Ztg,1968,92(2):41-50.
  • 3C1ewsFH,HugillW,GreenAT.Anexaminationofspecimensofsilicabrickworktakenfromaverticalretortandshowingevidenceofpronouncedalkaliattack[J].TransBritCerSoc,1940,33(1):337-344.
  • 4PandaJD,GoswamiG,SabuP,etal.CreeppropertiesofIndiansilicacokeovenbricks[C]//ProcofUNITECR’93,SaoPaulo,Brazil,1993:1205-1214.
  • 5PandaBK,SahuP,PandaJD.Investigationofusedsilicabricksintallcokeovens[C]//ProcofUNITECR’03,Osaka,Japan,2003:No21C-10.
  • 6ZamboniLA,CalihgarisMG,QuarantaNE.Silicabricksafterfifteenyearsinservice:Criticalstudy[J].Interceram,1997(3):162-166.
  • 7NaritaY,UedaH.Alterationofsilicabricksforcockovens[J].耐火物,1999(8):459-466.
  • 8王先平,周述祥,黄虎,李万众.湘钢JNX43-83型焦炉蓄热室技术改造[J].金属材料与冶金工程,2008,36(3):33-36. 被引量:1
  • 9李勇,薄钧,刘雄章.热风炉长寿与低蠕变Al2O3-SiO2系耐火材料的探究[J].耐火材料,2008,42(3):215-218. 被引量:10
  • 10郭治.焦炉蓄热室的传热模拟[J].燃料与化工,1990,21(3):13-18. 被引量:2

共引文献10

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部