摘要
通过研究硫酸铅渣的成分、性质、反应特征和开展协同处理过程的热平衡计算,结合工业试验,得到了硫酸铅渣配入比例在15%条件下的无烟块煤配入比例、渣型控制、氧料比控制等关键工艺参数条件,探索出了SKS炼铅法协同处理硫酸铅渣的最佳冶炼条件,以期进一步提高底吹炉处理硫酸铅渣的能力。
By studying the composition, properties and reaction characteristics of lead sulfate slag, heat balance calculation of synergistic treatment process was carried out.Combined with industrial experiments, the key process parameters such as proportion of anthracite lump coal, slag type control, and oxygen material ratio control were obtained when the proportion of lead sulfate slag was 15%.The optimum smelting conditions of SKS lead smelting process for synergistic treatment of lead sulfate slag were explored, so as to further improve the capacity of bottom blowing furnace to treat lead sulfate slag.
作者
黄安平
唐志波
佘国徽
HUANG An-ping;TANG Zhi-bo;SHE Guo-hui(Hunan Shuikoushan Nonferrous Metals Group Co.,Ltd.,Hengyang 421513,Hunan,China)
出处
《有色金属(冶炼部分)》
CAS
北大核心
2022年第9期179-183,共5页
Nonferrous Metals(Extractive Metallurgy)
基金
国家重点研发计划项目(2018YFC1903302)。
关键词
硫酸铅渣
SKS炼铅法
底吹炉
渣型
无烟块煤
热平衡
lead sulfate slag
SKS lead smelting process
bottom blowing furnace
slag type
anthracite lump coal
heat balance