摘要
低密度水泥浆常用泡沫和漂珠作为减轻材料,但泡沫和漂珠的一个共同缺陷是承压能力有限,这就给固井施工带来一定风险。通过大量实验,以颗粒紧密堆积为原则,复配出一种新型实心耐压减轻材料FXW。实验证明,减轻材料FXW与其它外加剂相容性好,浆体施工性能优良;FXW为实心减轻材料,能够承受井下高压,解决了漂珠和泡沫低密度水泥浆不能承压的问题;FXW低密度水泥石强度高,韧性好,可满足油井后期开发需求。
Foam and hollow micro-spheres are the widely used light-weight-additives (LWA) in low-density cement slurries, but both of them have low compressive strengths; therefore their use is sometimes risky. A new solid compression-resistant LWA, FXW was developed based on the"close packing of particles" principle through the field and laboratory experiments. It is shown that FXW has a good compatibility with other additives, and the slurries treated with FXW have excellent operation performances. Compare...
出处
《钻井液与完井液》
CAS
北大核心
2006年第6期50-51,85,共3页
Drilling Fluid & Completion Fluid
关键词
固井
水泥浆
低密度
减轻剂
well cementing
cement slurry
low-density
light-weight-additives