热水器不锈钢内胆孔蚀原因的研究 被引量:6

STUDY ON PITTING CORROSION OF STAINLESS STEEL FOR WATER HEATER TANK
下载PDF
导出
摘要 根据国内热水器不锈钢内胆孔蚀多发地区水质分析报告 ,研究了自来水的稳定性、Cl-、NaClO含量以及温度对不锈钢孔蚀趋势的影响 ,并从不锈钢内胆材质以及加工工艺分析了孔蚀集中发生在焊缝附近的原因 .实验证明热水器不锈钢内胆孔蚀是不锈钢成分和组织结构与特殊腐蚀介质。 A study on the influence of tap water stability,the Cl - and NaClO concentration,and temperature on pitting corrosion tendency of stainless steel was carried out with tap waters from several cities,where corrosion induced perforation of stainless steel water heaters was reported.Based on the perforation nearby the weldmenfs of the water tank and the experimental results,it follows that the pitting corrosion of stainless steel tank was induced by synergetic effect of many factors including the chemical composition and microstructure of the stainless steel, corrosive mediums and temperature.
出处 《腐蚀科学与防护技术》 CAS CSCD 北大核心 2001年第z1期526-530,共4页 Corrosion Science and Protection Technology
关键词 热水器 不锈钢 孔蚀 water heater,stainless steel,pitting corrosion
  • 相关文献

参考文献3

  • 1[3]吴荫顺.腐蚀实验方法与防腐蚀检测技术.北京:化学工业出版社,1996.87
  • 2[6]Fontana F G, Greene N D. Corrosion Engineering. McGrawHill Book Co., New York. 1967.51
  • 3[7]A约翰塞德赖克斯著,吴剑译.不锈钢的腐蚀.北京:机械工业出版社,1986.117

同被引文献9

引证文献6

二级引证文献14

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部