摘要
研究了B对过共晶Al-20Si合金中初晶Si的细化作用。结果表明,B对过共晶Al-Si合金初晶Si有较好的变质效果。初晶Si的尺寸先随B含量的增加而减小,当B的添加量为0.065%时达到最佳的细化效果,之后初晶硅的尺寸开始随B含量的增加而增大。
The modification of the primary silicon in hypereutectic Al-20wt.% Si alloy by boron has been investigated. The results show that boron addition can obviously modify the primary silicon in hypereutectic Al-20wt.% Si alloy. The size of the primary silicon decrease with the increase of boron addition content from 0 to 0.065 wt.%,and the minimum size of the primary silicon can be obtained at the boron addition content of 0.065 wt.%. But, the size of primary silicon increases if the boron addition content is co...
出处
《特种铸造及有色合金》
CAS
CSCD
北大核心
2008年第S1期140-142,共3页
Special Casting & Nonferrous Alloys