摘要 The distribution behavior of the HZB collector (a kind of long chain fatty acid) in the desilication system of bauxite flotation was studied. The results show that the collector tends towards froth products in the steps of the roughing, the first cleaning and the second cleaning, while towards the tailing product in the step of the scavenging, and in each job except scavenging the collector is mainly on the surface of solids. As for the froth product in the step of the scavenging, it is mainly in solution. To the tailing products of every step, it is mainly in the respective solutions. The collector added to the flotation system is mainly taken out by the last concentrate, by which the taken one occupies 65.2% of the whole, among which, 57.8% is by solid and 7.4% by solution, respectively. And the one by the last tail occupies 34.8% of the whole, among which, 8.8% is by solid and 26.0% by solution, respectively. The sum of the collector in the solution of the last concentrate and tailing is 33.4% of the amount of addition collector, and recycling the solutions will be in favor of decreasing the dosage of collector. The distribution behavior of the HZB collector (a kind of long chain fatty acid) in the desilication system of bauxite flotation was studied. The results show that the collector tends towards froth products in the steps of the roughing, the first cleaning and the second cleaning, while towards the tailing product in the step of the scavenging, and in each job except scavenging the collector is mainly on the surface of solids. As for the froth product in the step of the scavenging, it is mainly in solution. To the tailing products of every step, it is mainly in the respective solutions. The collector added to the flotation system is mainly taken out by the last concentrate, by which the taken one occupies 65.2% of the whole, among which, 57.8% is by solid and 7.4% by solution, respectively. And the one by the last tail occupies 34.8% of the whole, among which, 8.8% is by solid and 26.0% by solution, respectively. The sum of the collector in the solution of the last concentrate and tailing is 33.4% of the amount of addition collector, and recycling the solutions will be in favor of decreasing the dosage of collector.
出处 《Journal of Central South University of Technology》 2001年第2期125-129,共5页 中南工业大学学报(英文版)
基金 TheKeyProgramofthe 9thFive yearPlanofChina (96 112 0 1 0 1)
关键词 distribution of collector DESILICATION flotation of bauxite distribution of collector desilication flotation of bauxite
  • 相关文献

参考文献1

二级参考文献2

共引文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部