黄龙滩大坝的裂缝多达1000余条,自投入运行以来,曾进行过多次处理。简要介绍了1994年大规模处理的所用材料、工艺和质量控制以及处理效果。
There are more than thousand cracks occurred on the surface of Huanglongtan Dam and the work for blocking them has been done for three times since the dam was put into operation. Here, the treating materials and technology, quality control and result of the repairing work are described briefly.
出处
《湖北水力发电》
2001年第3期37-39,43,共4页
Hubei Water Power
关键词
黄龙滩大坝
裂缝处理
材料配比
质量控制
Huanglongtan Dam
crack treatment
mix proportion of materials
quality control