摘要 金、银丝不耐酸、碱、高温,不耐磨,按常规染整工艺加工,会出现严重褪色现象,使布面完全失去亮片光泽。金(银)丝/人造丝/锦氨混纺花边染整加工中,人造丝采用高反应性活性染料和5~10 g/L纯碱于温度40℃染色,同时控制皂洗pH<8;锦纶采用酸性染料于温度80~90℃染色,染液pH值控制在4.5以上,可确保金、银丝亮片不褪色,保持坯布织造时的光泽,且耐水洗牢度和耐摩擦牢度较好。 Owing to high alkalinity and high temperature in traditional wet processing,tinsel sequin will lose luster.In this paper,proper dyeing and finishing process for tinsel/rayon/nylon elastic lace is introduced.Rayon dyeing is carried out at 40 ℃ with high-activity reactive dyes and 5~10 g/L sodium carbonate,and the pH value of soaping is controlled below 8.Nylon dyeing is carried out at 80~90 ℃ with acid dyes and pH value of above 4.5.The new process can impart the elastic lace brilliant luster and good color fastness to washing and rubbing.
作者 陈怡珊
出处 《印染》 北大核心 2012年第5期24-25,共2页 China Dyeing and Finishing
关键词 染整 混纺织物 花边 dyeing and finishing blended fabric lace
  • 相关文献

同被引文献6

引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部