龟石水库灌区仁岩渡槽渗漏加固处理

Anti-seepage reinforcement and treatment for Renyan flume in irrigation area of Guishi reservoir
下载PDF
导出
摘要  贺州市龟石水库灌区仁岩渡槽经过30多年的运行,槽身渗漏造成钢筋锈蚀、槽壳外侧钢筋保护层混凝土脱落,伸缩缝防渗材料老化失效。介绍了防渗漏处理过程中,浆液及其配合比,对槽身伸缩缝等不同部位采取的各种施工工艺。 After 30 years of operation, the Renyan flume in the irrigation area of Guishi reservoir of Hezhou city had seen steel bar rust due to flume seepage, fall of bar_protective concrete, aging and abatement of anti_seepage material at expansion joint. A detailed introduction is made on the anti_seepage treatment that had been conducted for this flume, including the slurry and mix proportion, different construction technique for different positions such as flume body, flume shell, expansion joint water stop.
作者 何令祖
出处 《广西水利水电》 2004年第2期93-94,96,共3页 Guangxi Water Resources & Hydropower Engineering
关键词 龟石水库 渡槽 化学灌浆 渗漏 修补 伸缩缝 Flume chemical grouting seepage repair expansion joint
  • 相关文献

参考文献2

  • 1广西水利科学研究所.贺州龟石水库灌区仁岩渡槽堵漏处理[R].南宁:广西水利科学研究所,2002..
  • 2黄国兴 陈改新.水工混凝土建筑物修补技术及应用[M].北京:中国水利水电工业出版社,2002,3..

共引文献18

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部