管节点与船舶甲板结构中疲劳裂纹扩展方向的研究

PROPAGATION DIRECTION STUDY OF FATIGUE CRACKS IN TUBULAR JOINTS AND SHIP DECK STRUCTURES
下载PDF
导出
摘要 线性断裂力学中研究裂纹的扩展通常用应力强度因子的断裂准则,但是对复合型裂纹,应力强度因子理论就发生了困难。本文用光弹性方法求得裂纹前缘的应力强度因子,然后用应变能密度因子理论研究了船舶大开口舱口角隅处疲劳裂纹和T型管节点热点处表面裂纹的扩展规律和方向。 The fracture criterion of Stress Intensity Factor is usually applied to study the propagation of fatigue cracks. However, it would meet difficulties while it is used to study the growth of the cracks that are subjected to mix mode loading. In the present paper, the photoelasticity experiment and the strain energy density factor theory are combined to study the propagation direction of fatigue cracks under mix mode loading. Two growth profiles that includes a surface crack at hot spots in the tubular T joints and two propagation loci of fatigue cracks at the hatch corner in two types of large opening deck models have been obtained with satisfactory results.
作者 钱仍 责力
机构地区 上海交通大学
出处 《海洋工程》 CSCD 北大核心 1996年第1期82-88,共7页 The Ocean Engineering
关键词 裂纹扩展方向 疲劳应变能 密度因子 propagation direction of crack, fatigue, strain energy density
  • 相关文献

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部