摘要
介绍了炉膛进水后再沸炉的损坏和检测情况,分析了Cr5Mo炉管损伤的程度,制定出合理的处理方法,为解决类似问题提供了借鉴。
The damage and inspection situation of reboiler furnace firebox after water admission were recommended. The damage degree of Cr5Mo furnace tube was analyzed. The reasonable handling method was made. This experience could be used for reference to similar problems.
出处
《石油化工设备技术》
CAS
2004年第1期32-35,共4页
Petrochemical Equipment Technology
关键词
CR5MO
炉管
无损检测
Cr5Mo, Furnace tube, Nondestructive examination