期刊文献+

芳纶纤维增强橡胶密封板材的配方设计 被引量:4

Formulating of Recipe of Aramid Fiber Reinforced Rubber Sheet
下载PDF
导出
摘要 以拉伸强度为指标 ,利用均匀设计法对芳纶纤维增强橡胶密封板材进行配方设计 ,优选得到了理想的配方。采用模压工艺制备出了优选配方的密封板材 ,并作了性能测试。试验结果表明 ,其各项性能均达到了国家标准 (报批稿 )的要求。 The formulating of recipe of the no-asbestos sealing material filled with Aramid fiber was carried out by the uniform design method, according to the results of the transverse tensile test. The sealing material with perfect recipe was manufactured by molding process. The gasket performance tests were conducted, and there is good agreement between the test results and the indexes prescribed in the Chinese national standard.
出处 《润滑与密封》 EI CAS CSCD 北大核心 2004年第4期95-96,111,共3页 Lubrication Engineering
关键词 芳纶纤维 密封板材 均匀设计法 配方设计 拉伸强度 Design Fiber reinforced materials Rubber molding Seals Tensile testing
  • 相关文献

参考文献13

  • 1.中华人民共和国国家标准.管法兰用非金属平垫片技术条件(报批稿).[S].,..
  • 2金振国.号召国际性禁止使用石棉[J].江苏职业卫生通讯,2000(3):5-6. 被引量:1
  • 3Keith R, Watson, Arnold F. Elastomer reinforcement with short Kevlar aramid fiber for wear applications. Rubber world, 1988,208 (8): 20.
  • 4Karlheinz Hillermeier. Prospects of Aramid as a Substitute for Asbestos [J]. Textile Research, 1984, (9):575~580.
  • 5Rndall JRigers, Richard P Foster, Kimberly L Waastler. Considerations in the formulation of gasket materials [ J ] . Tap - pi. ,1991 (9) : 127~132.
  • 6芦田道夫.增强纤维(短纤维)[J].橡胶译丛,1992,(4):38-45.
  • 7Lindeman. Asbestos free gasket forming compositions [ P].USP: 4330422, 1982.
  • 8方开泰.均匀设计与均匀设计表[M].北京:科学出版社,1996..
  • 9方开泰,马长兴.正交与均匀试验设计.北京:科学出版社,2001.
  • 10谢苏江 蔡仁良.一种用纤维增强的软木橡胶密封材料及其制备工艺[P].中国:中国发明专利,C1110300A.1994-11-04.