在“THERMECMASTOR -Z”热加工模拟试验装置上模拟了加热温度、保温时间、变形速度等对含钒高碳钢组织的影响 ,分析了不同变形温度下氮浓度对析出物的影响。
The effects of reheating temperature,holding time and deformation speed on the structure of high carbon steel are simulated at the thermo-working simulator 'THERMECMASTOR-Z'and impact of nitrogen concentration under the different deformation temperatures on the precipitation is analyzed.
出处
《武钢技术》
CAS
2004年第5期19-22,共4页
Wisco Technology
关键词
微量钒
高碳钢
析出物
trace amount of vanadium
high carbon steel
precipitate