铸模焙烧温度对Plat铸造陶瓷全冠适合性的影响 被引量:1

Casting Model Burnout Temperature Effect on the Adaption of Plat Castablc Ceramic Crowns
下载PDF
导出
摘要 用600C、700C、800C、900C4种铸模焙烧温度铸造Plat陶瓷冠40个,每组10个,测试并比较全冠各部位,各组全冠的适合性,结果表明各组间全冠的适合性无显著性差异,其边缘浮升量均为250μm左右。实验测得同一冠的龈缘及(牙合)面粘固剂厚度较接近,且远较轴壁处厚。 In this study the author investigated and compared the adaption of Plat castable ceramic crowns Which cast by varies model burnout temperature (600℃ . 700℃. 800 ℃ . 900℃ ). And the results indicated there were no significant differences of crown fit among fourgroups (P > 0. 05). The average marginal opening were 249. μm. 261μm. 267. 3μm. 265. 5μm tespectively, the cement thickness of occlusal and marginal parts were simila.and fairly more than that of axial parts.
出处 《口腔材料器械杂志》 1994年第1期14-15,19,共3页 Chinese Journal of Dental Materials and Devices
关键词 全冠 适合性 PLAT铸造陶瓷 龈缘 粘固剂 影响 部位 铸模 厚度 castalbe ceranic crown castingu model burnout temperature adaption
  • 相关文献

参考文献1

二级参考文献8

  • 1Hobo S,et al.Castable apatite ceramics as a new biocompatible restorative material.I. Theoretical considerations. Quintessence International . 1985
  • 2Grossman DG.Cast glass ceramics. Dental Clinics of North America . 1985
  • 3Gardner RM.Margins of complete crowns-literature review. The Journal of ProsThetic Dentistry . 1982
  • 4Rusayama T. et al.Relief of resistance of cement of full cast crowns. The Journal of ProsThetic Dentistry . 1964
  • 5Mclean JW,et al.The estimation of cement film thinkness by an in vivo technique. British Dental Journal . 1971
  • 6Grajower R,et al.Improving the fit of crowns with dic spacers. The Journal of ProsThetic Dentistry . 1989
  • 7Campagni WV,et al.Effect of die spacer on the seating of complete cast gold crowns with grooves. The Journal of ProsThetic Dentistry . 1986
  • 8Van Nortwick WT,et al.Effect of internal relief ,vibration, and venting on the vertical seating of cemented crowns. The Journal of ProsThetic Dentistry . 1981

同被引文献8

  • 1Randa Diwan, Yousef Talic, Noura Omar, et al. Pattern waxes and inaccuracies in fixed and removable partial denture castings. J Prosthet Dent, 1997,77(5) = 553 -555.
  • 2Thompson VP, Williams EF, Bailey WJ. Dental Resins with Reduced Shrinkage During Hardening. J Dent Res, 1979,58(5) : 1522 - 1532.
  • 3Takahashi J, Kitahara K, Wangxue, et al. Resin pattern material with low polymerization shrinkage. Int J Prosthodont, 1999 ,t2(4) : 325 - 329.
  • 4Nourallah H, Hammad I. Marginal castability of two different materials (a comparative study). Egypt Dent J, 1994, 40( 1 ) : 649 - 652.
  • 5May KB, Russell MM, Razzoog ME, et al. Precision of fit: the Proeera Alleerarn crown. J Prosthet Dent, 1998, 80(4) : 394 -404.
  • 6Stevens L. Model investing method of FPD construction: its accuracy. Dent Mater, 1986, 2(4) : 166.
  • 7陈贤福,盛列平.GC铸型树脂在铸造桩核中的应用[J].口腔材料器械杂志,2000,9(1):18-19. 被引量:1
  • 8常中炎,王忠义,毛勇,艾绳前.不同种类的熔模材料对玻璃陶瓷全冠精度的影响[J].临床口腔医学杂志,2001,17(4):276-277. 被引量:4

引证文献1

二级引证文献2

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部