摘要
针对新投产铸机生产包晶钢表面纵向裂纹多的现状,分析原因并进行工艺参数优化、工艺操作改进,有效地提高了铸坯表面质量合格率。
The process parameters and operation have been optimized based on the analysis on longitudinal surface crack of peritectic steel slab cast with the new caster. The slab surface quality has been greatly improved.
出处
《连铸》
2005年第1期31-33,共3页
Continuous Casting