摘要
真空熔渣电阻炉冶炼低微碳铬铁是利用熔渣导电,电阻发热使炭素铬铁和铬矿熔化,在1923—1973K、真空度为1333—266GPa下进行液态脱碳,从而获得低微碳铬铁。本文从理论上和冶炼设备上对其可行性进行了探讨。
The process of production of low and extra low carbon ferrochromi urn is melting the carbon fcrrochromium and chromite by conduction of molten slag and resistance heat, undergoing liquid decarbonization with temperature of 1923—1973K, vacuity of 1333—2666Pa, gaining the products finally. This paper also discusses the feasibility about its theories and equipments.
出处
《铁合金》
北大核心
1993年第1期19-20,6,共3页
Ferro-alloys