摘要
生产中配料和工艺不当,以及氯氧镁水泥水化产物本身的耐水性差和在硬化及使用过程中产生并发展的显微裂纹是引起这种水泥常见缺陷的主要原因。本文就上述因素的影响情况进行了讨论,并提出了相应的解决措施。
Improper mix and technology in the production of sorel cement, poor in water resistane of the hydrated products, and microfissure occussed and develofed in the hardening process and use are the main causes for the defects of sorel cement commonly found. In this pa- per, influence of the above factors is discussed, and corresponding measuses for solution are proposed.
出处
《中国建材科技》
1993年第4期5-9,共5页
China Building Materials Science & Technology
基金
浙江省自然科学基金