316不锈钢原位质子辐照疲劳过程中的声频内耗

Acoustic Internal Friction of 316 Stainless Steel in Fatigue Process with in Situ Proton Irradiation
下载PDF
导出
摘要 316不锈钢原位质子辐照下疲劳过程中的声频内耗用弯摆在333~573K温区和应变振幅为10 ̄(-4)量级下进行了研究。结果表明,有质子辐照的疲劳过程中的内耗在较大应变振幅下是与振幅有关的内耗。用应变振幅(2.92~4.39)×10 ̄(-4)疲劳时,在373~403K有微弱的内耗峰出现。有质子辐照疲劳中的内耗明显小于无质子辐照疲劳中的内耗。 Acoustic internal friction of 3 1 6 stainless steel in fatigue process with in situ proton irradiation was studied using flexural pendulum within temperatures 3 3 3~573K and the strain amplitude order is of 10-4.The results show that internal friction in fatigue process with in situ proton irradiation is strain amplitude dependent. The small internal friction peaks in the temperature range of 373~403 Koccurred in fatigue process with the strain amplitudes of(2.92~4.39)×10-4.And the internal frictions are obviously lower in fatigue process with in situ proton irradiation than those without proton irradiation.
出处 《材料科学与工艺》 CAS CSCD 北大核心 1994年第3期12-16,共5页 Materials Science and Technology
关键词 不锈钢 声频内耗 疲劳 质子辐照 proton irradiations,acoustic internal frictions fatigue
  • 相关文献

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部