期刊文献+

固相反应合成磷酸四钙的物相演变 被引量:4

Phase Transition of Synthesizing Tetracalcium Phosphate in a Solid-state Reaction
下载PDF
导出
摘要 采用TGA-DSC、FTIR及XRD等方法研究了固相反应法合成磷酸四钙(TTCP) 的物相演变过程.结果表明,1200℃以上物相变化与CaO-P2O5-H2O)的高温相图基本一致, 1200℃以下的物相变化为绘制CaO-P2O5-H2O低温相图提供重要数据;通过揭示固相合成 TTCP物相演变的全过程,为制备出纯TTCP这一重要的磷酸钙骨水泥组成材料提供重要理 论依据. The phase transition course of synthesizing tetracalcium phosphate in a solid-state reaction was investigated by TGA-DSC, XRD and FTIR. The results show that the phase transformations occurring over 1200 degrees C are consistence with the high temperature phase diagram of CaO-P2O5-H2O. In view of lack of the low temperature phase diagram, the phase transitions below 1200 degrees C can offer significant data to draw it; understanding the whole course of phase evolution contributes to optimum the synthesizing process to get pure TTCP, the most important biomaterial in the field of calcium phosphate cement.
出处 《无机材料学报》 SCIE EI CAS CSCD 北大核心 2005年第2期317-322,共6页 Journal of Inorganic Materials
基金 国家自然科学基金(50002008)教育部"跨世纪优秀人才培养计划"(2001年度)西安交通大学博士论文基金
关键词 磷酸四钙(TTCP) 固相反应 物相演变 生物陶瓷 tetracalcium phosphate solid-state phase reaction phase transitions bioceramic
  • 相关文献

参考文献12

  • 1戴红莲,闫玉华,王友法,李世普,江昕.磷酸四钙粉末的制备研究[J].硅酸盐通报,2002,21(4):56-59. 被引量:9
  • 2郭大刚,付涛,徐可为.短棒状纳米羟基磷灰石的湿法合成及表征[J].硅酸盐学报,2002,30(2):189-192. 被引量:32
  • 3Doi Y, Shimizu Y, Moriwaki Y, et al. Biomater., 2001, 22 (8), 847-854.
  • 4Gbureck U, Probst J, Thull R. Biomole. Engin., 2002, 19 (2-6), 51-55.
  • 5Sargin Y, Kizilyalli M, Telli C, et al. J. Euro. Cera. Soc., 1997, 17: 963-970.
  • 6Brown W E, Chow L C. Ameraican patents, 4518430. 985-30-21.
  • 7刘义荣 盂爱英 薛淼.牙体牙髓牙周病学杂志,1996,9(2):110-112.
  • 8Tronstad L. Clinical Endodontics, the first edition, New York: Thiem Medical Publishers, 1991. 110-120.
  • 9Cox C F, Beroenholtz G, Heys R. J. Oral. Pathol., 1985, 14: 156-160.
  • 10Feng H L, Liao C J, Chen K S, et al. Mater Sci Eng C, 2000, 13: 97-104.

二级参考文献13

  • 1关英.岩石矿物分析[M].北京:地质出版社,1991.158-159.
  • 2张士成(ZHANG Shicheng). 羟基磷灰石超微粉对癌细胞作用初探[D]. 武汉:武汉工业大学(Wuhan: Wuhan University of Technology), 1996. 21-29.
  • 3LIU Deanimo. Fabrication of hydroxyapatite ceramic with controlled porosity.[J]. J Mater Sci: Mater Med. 1997, 8 (4):227-232.
  • 4LI Yubao, DE Groot K, DE Wijn J, et al. Morphology and composition of nanograde calcium phosphate needle-like crystals formed by simple hydrothermal treatment [J]. J Mater Sci: Mater Med, 1994,5 (6-7):326-331.
  • 5路迪民(LU Dimin). 金属学(Metallography) [M]. 西安:西北大学出版社(Xi'an: Northwestern University Press), 1994. 84-91.
  • 6DOREMUS R H. Review Bioceramics [J]. J Mater Sci, 1992, 27(1-3): 285-297.
  • 7TERAOKA K, ITO A, ONUMN K, et al. Bending strength of synthetic OH-carbonated hydroxy apatite single crystals [J]. J Biomed Mater Res, 1997, 34(2): 269-272.
  • 8HALOUANI R, BERNACHE D, CHAMPION E, et al. Microstructure and related mechanical properties of hot pressed hydroxyapatite ceramics[J]. J Mater Sci: Mater Med, 1994 (5):563-568.
  • 9ROYER A, VIGUIE J C, HEVGHEBAERT M, et al. Stoichiometry of hydroxyapatite: influence on the flexural strength[J]. J Mater Sci: Mater Med, 1993, 4(1):76-82.
  • 10WANG M, JOSSPH R, BONFIELD W. Hydroxyapatite-polyethylene composites for bone substitution: effects of ceramic particle size and morphology[J]. Biomater, 1998(19):2 357-2 366.

共引文献39

同被引文献38

引证文献4

二级引证文献31

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;