摘要 在实验室条件下对用丙烯腈-苯乙烯共聚物在硫酸存在下的水解磺化产物(HSAS)处理的泥浆性能进行了评定。HSAS处理的泥浆有较小的滤失性,较好的耐盐和抗高温性。 The performane of a simultaneous hydrolysis and sulfonation product of acrylnitnle-styrene copolymer, HSAS,as clay drilling mud stabilizer is evaluated in laboratory.0.3-0.5% HSAS(AN:St=90:10,prepared in 96% sulfuric acid at 100℃) in fresh water mud and 0.7% HSAS in 3% NaCl mud reduce their filtrate loss at ambient temperature down to 15ml.0.3% HSAS-treated fresh water mud maintains its filtrate loss of 22ml at 60℃ after thermal aging at 180℃ over 12 hrs.This HSAS-treated fresh water mud has increasal plastic viscosity and yield stress.The influence of copolymer composition(ratio AN/St) and sulfuric acid concentration for hydrolysis/sulfonation is also investigated. Most HSAS samples are shown to be strong viscosifier.
出处 《油田化学》 CAS CSCD 北大核心 1994年第4期292-295,共4页 Oilfield Chemistry
关键词 丙烯腈 苯乙烯 共聚物 稳定性 钻井泥浆 Product of Hydrolysis/Sulfonation of Acrylnitrite/Styrene Copolymer(HSAS),Drilling Mud Stabilizer,Filtrate-Loss Control,Salt Tolerency,High Temperature Resistance,Laboratory Performance Evaluation
  • 相关文献

参考文献3

二级参考文献1

  • 1张维邦,卢沛女.泥浆稳定剂Ⅰ——部分水解聚丙烯腈的研究[J]石油钻采工艺,1981(02).

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部