摘要
共接Nd3+离子改善了Cr:ZnWO4单晶质量,提高了激光效率。室温下用红宝石激光泵浦,在φ6×19mm的晶棒中,获得0.95μm的激光脉冲,最大输出能量达1.62mJ,泵浦斜率效率为0.79%。
Codoped Nd3+ ion improved the quality of Cr:ZnWO4 single crystal and raisedits lasing efficiency.Laser pulse at wavelength 0.95 μm was generated with a 6 mmdiameter,19 mm long rod,which was pumped with a ruby laser The maximum outputenergy is 1.62 mJ and the slop efficiency is 0.79 %.
出处
《中国激光》
EI
CAS
CSCD
北大核心
1994年第9期721-723,共3页
Chinese Journal of Lasers