Effect of Produced Fluid on the Wear Behavior of Grade D Sucker Rod and N80 Type Tubing 被引量:2

Effect of Produced Fluid on the Wear Behavior of Grade D Sucker Rod and N80 Type Tubing
下载PDF
导出
摘要 Inuestigated wear tests of grade D sucker rod and N80 tubing with a produced liquid are the effect of the water cut of produced liquid on the wear rate and the wear coefficient of the friction pair. And presented here is a comparison of tribological performance of tubing/sucker rod with sprayed tubing/sucker rod and tubing/sprayed sucker rod. The results show that one of the main reasons for wear failure between the sucker rod and the tubing is a high water cut of the produced liquid. The wear rate increases greatly when the water cut ranges from 70% to 85%, and increases gradually when the water cut is less than 70% or more than 85%. The higher the water cut is, the greater the wear rate will be. SEM (scanning electron microscope) micrographs show that the worn surface of the tubing is smoother, with shallow grooves, when the water cut is 55%; when the water cut is 95%, there are broader and deeper grooves on the worn surface. The results also show that the wear rate of the sprayed wear-resistant coating of sucker rod/tubing is less than that of the unsprayed sucker rod/tubing. Inuestigated wear tests of grade D sucker rod and N80 tubing with a produced liquid are the effect of the water cut of produced liquid on the wear rate and the wear coefficient of the friction pair. And presented here is a comparison of tribological performance of tubing/sucker rod with sprayed tubing/sucker rod and tubing/sprayed sucker rod. The results show that one of the main reasons for wear failure between the sucker rod and the tubing is a high water cut of the produced liquid. The wear rate increases greatly when the water cut ranges from 70% to 85%, and increases gradually when the water cut is less than 70% or more than 85%. The higher the water cut is, the greater the wear rate will be. SEM (scanning electron microscope) micrographs show that the worn surface of the tubing is smoother, with shallow grooves, when the water cut is 55%; when the water cut is 95%, there are broader and deeper grooves on the worn surface. The results also show that the wear rate of the sprayed wear-resistant coating of sucker rod/tubing is less than that of the unsprayed sucker rod/tubing.
出处 《Petroleum Science》 SCIE CAS CSCD 2005年第2期116-118,共3页 石油科学(英文版)
关键词 Sucker rod WEAR water cut sprayed wear-resistant coating Sucker rod, wear, water cut, sprayed wear-resistant coating
  • 相关文献

同被引文献14

引证文献2

二级引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部