摘要
用浸渍法制备了Fe3+-TiO2/SiO2负载型光催化剂并进行了光催化降解气相中甲苯的实验研究。结果表明,Fe3+掺杂量(nFe3+/Ti4+)为0.3%时光催化降解甲苯的效率最高。水气的存在提高了Fe3+-TiO2/SiO2负载型催化剂的光催化活性,但使Fe3+-TiO2纳米粉的光催化活性降低;而O2的存在使Fe3+-TiO2纳米粉和Fe3+-TiO2/SiO2负载型催化剂的催化活性均有所降低。动力学研究表明,光催化降解气相中甲苯的动力学为一级反应。
Photocatalytic degradation of toluene using Fe 3+-TiO_2/SiO_2 thin film photocatalysts prepared by means of impregnation method has been performed in gas phase. The photocatalytic activity of prepared catalysts reach the maximum at the optimal content n_ Fe 3+/n_ Ti 4+=0.3%. With increasing water vapor concentration, the photocatalytic activity of Fe 3+-TiO_2/SiO_2 increases, while TiO_2 nanoparticles activity declines. For both them, the presence of O_2 results in photocatalytic activity decrease. The experimental results indicate that the kinetics of toluene degradation can be described by one-order reaction equation.
出处
《黑龙江大学自然科学学报》
CAS
北大核心
2005年第3期305-308,共4页
Journal of Natural Science of Heilongjiang University
基金
国家自然科学基金资助项目(20431030
20301006)
黑龙江省杰出青年科学基金资助项目(2002)
黑龙江省自然科学基金资助项目(B0305)
黑龙江省科学技术计划项目(WB02103)
黑龙江省教育厅科学计划项目(10541171)
关键词
光催化降解
铁掺杂TiO2
甲苯
photocatalytic degradation
Fe-doped TiO_2
Toluene