期刊文献+

湿法纺丝中凝固成形和拉伸对聚丙烯腈原丝结构和性能的影响(英文) 被引量:6

The Effect of Coagulation and Stretch on the Structure and Properties of PAN Precursor by Wet Spinning
下载PDF
导出
摘要 凝固成形和拉伸是原丝生产过程中两个十分关键的工序,它们对聚丙烯腈原丝的结构和性能有着重要的影响。纤维的拉伸强度在凝固成形过程中受到凝固浴浓度、温度和负拉伸的影响,同时在纤维的拉伸中拉伸的倍数、温度和介质等也影响着纤维的结构和性能。 Coagulation and stretch are two crucial working procedures during precursor fabrication, which play important roles in precursor structure and performance. The fiber tensile strength is affected by concentration, temperature and minus stretch during coagulation, while the fiber structure and performance are obviously in- fluenced by stretch temperature, medium and ratio.
出处 《合成纤维》 CAS 北大核心 2005年第5期24-28,共5页 Synthetic Fiber in China
关键词 凝固 拉伸 聚丙烯腈原丝 拉伸强度 coagulation, stretch, PAN precursor, tensile strength.
  • 相关文献

参考文献11

  • 1M R Moghbel,N Mohammad, et al. Wet spinning of low gel content SBR/PMMA core/shell particles dispersed in a good solvent for the shell Polymer,2003,44,4011 ~4019.
  • 2Han M J,Bummer P M,et al. Phase transitions of polysulfone solution during coagulation. Polymer, 1995,24(36),4711 ~4714.
  • 3Edie D D.The effect of processing on the structure and properties of carbon fibers. Carbon, 1998, 36(4), 345~362.
  • 4WuGM.聚合物材料的生产和加工[M].北京:中国纺织工业出版社,1997.133-134.
  • 5E R Alieva, Yu P Kozhernikov, et al. Vlolkna, 1990.5,6
  • 6Knudsen J P.The influence of coagulation variables on the structure and physical properties of an acrylic fiber. Textile Research Journal,1963,33,13~20.
  • 7乔福牛.二甲基亚砜一步法碳纤维用聚丙烯腈原丝生产工艺[J].合成纤维工业,1995,18(4):19-23. 被引量:10
  • 8董纪震.合成纤维生产和加工[M].北京:中国纺织工业出版社,1995.428-429.
  • 9Johnson D J.Structure property relationships in carbon fibers.J Phys D:Appl Phys, 1987,20(3),287~291.
  • 10WangYX.[D].山东大学,2003.