将0Cr12Mn5Ni4Mo3Al钢于盐炉中分别在1 000、1 050及1 100 ℃×40 min条件下进行固溶处理后做-78 ℃×4 h冷处理及520 ℃×2 h时效处理。然后进行拉拉疲劳试验。
The solution treatments to 0Cr12Mn5Ni4Mo3Al were carried out in salt furnace under the condition of 1 000,1 050 and 1 100 ℃×40 min respectively. Then the cold treatments under the condition of -78 ℃×4 h and 520 ℃×2 h were followed. Tensile fatigue tests were finished finally.