摘要
本文利用粉煤灰、CNC双掺技术进行了防腐溶液、混合溶液浸泡试验,结果表明:普硅水泥抗蚀系数0.74~0.78,而防腐试件达1.0以上.并介绍了掺加优质粉煤灰、防腐剂对混凝土新拌及硬化后性能的影响,得出了防腐混凝土抗渗、抗冻等良好的物理力学性能的结论.
Fly-ash and corrosion preventing admixture are used in marinating tests with corrosion preventing solution and mixed soulation.We also introduce the influence of mixed fly-ash and corrosion preventing admixture on fresh and hydrated concrete.Based on the tests,we conclude that corrosion preventing concrete has favorable physical and mechanical performance.
出处
《混凝土》
CAS
CSCD
北大核心
2005年第6期84-86,共3页
Concrete
基金
建设部科技发展项目(03-02-09)
山东省科技攻关项目(031090162)
关键词
抗蚀系数
防腐溶液:
混合溶液
粉煤灰
防腐剂双掺:
防腐混凝土
<Keyword>coefficient of corrosion prevention
corrosion preventing solution
mixed solution
mixed use of fly-ash and corrosion preventing admixture
corrosion preventing concrete