摘要 用镍精矿-活性阳极泥-亚硫酸方法,研究了镍电解阳极液除铜效果;通过正交实验,查明了影响残铜量和mcu/mNi2个指标的主要因素和次要因素;得出最佳工艺条件是:镍精矿的质量浓度为0.30g/L亚硫酸体积分数为15.0mL/L阳极泥质量浓度为3.30g/L阳极泥活度为30%,反应温度为85℃,起始pH值为3.5,反应时间为40min。 The remove of copper from anode solution in nickel ectrolyte has been studied usingthe nickel concentrate-activited anode slime-sulfurous acid.The main factors to affect bothcopper content remaining in the solution and ratio of mCu/mNi the slag have been ascer-tained by means of orthogonal experinient.It is found that the best condition is as follows :nickel concentrate 0. 30 g/L,sulfurous acid 15.0 mL/L,anode slirne 3.30 g/L, activity ofanode slime 30%,temperature of reaction 85℃ starting pH 3.5,time of reaction 40 min。
出处 《中南工业大学学报》 CSCD 1995年第1期56-60,共5页 Journal of Central South University of Technology(Natural Science)
基金 国家"八五"科技攻关计划基金
关键词 镍矿 除铜 正交实验 镍电解液 decopper orthogonal experiment nickel electrolyte
  • 相关文献

同被引文献20

引证文献4

二级引证文献10

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部