摘要
铬渣加工成-200目均匀样品,(1+10)H_3PO_4为溶取剂.密封.经0.12~0.14MPa压力,121℃高温处理30min。此法可溶取铬渣中全量Cr(Ⅵ).不影响Cr(Ⅵ)的价态形式,并可消除Fe(Ⅲ)对Cr(Ⅵ)测定的干扰。
The chromium sludge is the solid waste from manufacture of Na_2CrO_4.The sample is processed to 200 mesh and homogenized. The total Cr(Ⅵ)in chromium sludge can be extracted in theextraction condition of 30 min. 1+10 H_3PO_4,sealed,0.12~0.14 MPa, 121℃.