摘要
本文应用地产原料劣质透辉石试制低温快烧釉面砖。烧成温度在1030~1100℃范围内.烧成周期为50~120min,吸水率19~21%;还试制了高遮盖乳浊釉,釉面白度可达78℃以上。
Using native inferior diopside as raw material,low-temperature and quick-senteimg glazed tile is devcloped.The sentewng temperature is ranged from 1030 to 1100 degree centigrade;sentering period,from 50 to 120 minutes;soid glaze ,with whiteness over 78 degree,is prodeced.