期刊文献+

Al-Fe-V-Si快速凝固热强铝合金中“块状相”的产生条件 被引量:5

FORMATION CONDITIONS OF MASSIVE PHASE IN RAPIDLY SOLIDIFIED Al-Fe-V-Si ALLOY
下载PDF
导出
摘要 通过快凝试验和电镜观察,对Al-Fe-V-Si合金中块状相的产生条件进行了分析.结果表明,合金中块状相产生的温度范围为1173-1103K,当熔体在该温度区间的冷却速度临界冷却速度,而快凝开始后的时形成块状相加微胞晶的快凝缺陷组织,当在整个快凝过程中时,则形成块状相加粗胞晶的快凝缺陷组织. An analysis for the formation conditions of the massive phase in Al-Fe-V-Si alloy was carried out by RS tests and TEM observations. The results show. the temperature range in which the massive phase occurs in is 1173-1103 K. The mixed structure of massive phase and microcellular will occurs when the cooling rate of the melt (the critical cooling rate) in the above temperature range and the cooling rate after RS starting.And the mixed structure of massive phase and coarse cellular will occurs when during whole RS process
机构地区 郑州工学院
出处 《金属学报》 SCIE EI CAS CSCD 北大核心 1995年第7期B295-B299,共5页 Acta Metallurgica Sinica
基金 国家863高技术资助
关键词 快速凝固 凝固温度 铝合金 显微组织 rapid solidification, solidification temperature, cooling rate, Al-Fe-V-Si alloy
  • 相关文献

参考文献1

  • 1汤亚力,硕士学位论文,1990年

同被引文献3

引证文献5

二级引证文献14

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部