摘要
聚乙烯醇装置中的乙酸精馏塔的工况条件,选择不锈钢、钛和脱氧钢3大类7种材料进行实验室和现场的大量试验,并对3类材料在乙酸中的腐蚀机理进行分析,提出了一个新的选材方向。
Acetic acid rectification tower(ART)is a major piece of equipment in polyvinyl alcoholunits,Currently,it is usually made of deoxidized copper. Because ART is subject to corrosion,thenormal operation of production has been frequently interrupted.in this paper,the authors selectseven kinds of materials of three categories of stainless steel,Ti and deoxidized copper to carryout field as well as labaratory experiments,analysis on the cause of corrosion,and put forward anew way of material option for ART.
出处
《石油化工》
CAS
CSCD
北大核心
1995年第9期642-642,共1页
Petrochemical Technology
关键词
乙酸
精馏塔
腐蚀
材料
stainless steel,Ti,deoxidized copper,corrosion,acetic acid rectification tower