摘要
通过测定试样经过3600小时后的次结晶度和后期收缩率,探讨了注射成型过程中冷却时间、注射速率和模具温度对聚酰胺1010(PA1010)制品尺寸稳定性的影响。
Abstract The effects of parameters (injection rate, mold temperature and cool time) on dimensional Stability of part of polyamide1010 (PA1010) were discussed by the testing analysis ofafter-crystallinity and after-shrinkage of the samples which were tested for 3600 hours.
出处
《塑料》
CAS
CSCD
1995年第2期45-48,共4页
Plastics