摘要
在1273~1523K的温度和10-3~100s-1的应变速率范围内研究了微量元素B,Mg对固溶有Cr,V合金元素的TiAl金属间化合物热变形性能的影响,计算并建立了相应的热变形方程和热加工图,确定了实验合金的动态再结晶峰应力.结果表明:B,Mg的加入提高了TiAlCrV合金的形变激活能,尤其是Mg的加入能显著改善TiAlCrV金属间化合物的热加工性能.
The effects of B and Mg on the hot deformation of TiAl intermetallic compound hsvebeen Studied in the present peper. The results show that the addition of B,Mg can increasethe deformation activation energy of TiAlCrV alloy and the hot workability of TiAJCrV alloy can be improved remarkedly by Mg.
出处
《西安工业学院学报》
1995年第3期197-203,共7页
Journal of Xi'an Institute of Technology
关键词
金属间化合物
变形分析
热变形
TIAL
硼
镁
intermetullic compound structure deformation analysis thermadynamic charts hot workability map