Ti—6Al—4V合金微动磨损的表面防护 被引量:5

Surface Protection Technique Against Fretting-Wear of Ti-6Al-4V Titanium Alloys
下载PDF
导出
摘要 分析对比了Ti-6Al-4V合金经喷丸后抛光、火焰喷涂Cu涂层、等离子喷涂锡青铜、Cu-Ni-In和WC/Co—I涂层、爆炸喷涂WC/Co-Ⅱ、Ni-60和化学镀镍磷镀层等处理后,在室温和500℃下的抗微动磨损性能。结果表明:WC/Co-Ⅰ涂层有较好的综合防护效果. Abstract: Shotting-peen, fire-sprayed Cu coatings, plasma-sprayed Sn-bronze, Cu-Ni-In and WC / Co-I coatings, explode-sprayed WC / Co-Ⅱ and Ni-60 coatings and chemical planting Ni-P are investigated and compared for the performances of several surface protective treatments againet fretting-wear of Ti-6Al-4V titanium alloys in room-temperature and 500℃.It shows that plasma-sprayed WC / Co-I has good integrative protective performance.
出处 《稀有金属材料与工程》 SCIE EI CAS CSCD 1995年第4期53-58,共6页 Rare Metal Materials and Engineering
  • 相关文献

参考文献1

  • 1翟金坤,黄子勋编.化学镀镍[M]北京航空学院出版社,1987.

同被引文献27

  • 1刘道新,何家文.经不同表面改性处理的钛合金的微动疲劳和微动磨损行为对比研究[J].摩擦学学报,2005,25(1):13-17. 被引量:29
  • 2DaoxinLIU,XiaodongZHU,BinTANG,JiawenHE.Fretting Fatigue Improvement of Ti6Al4V by Coating and Shot Peening[J].Journal of Materials Science & Technology,2005,21(2):246-250. 被引量:2
  • 3李东紫.微动损伤与防护技术[M].西安:陕西科学技术出版社,1992.288-320.
  • 4戴振东 薛群基 等.摩擦磨损过程的热力学模型[J].自然杂志,1998,20(40):220-228.
  • 5张永康.铝合金激光冲击强化抗疲劳特性的研究[M].南京:南京航空航天大学出版社,1996..
  • 6Hurricks P L.Wear[J],1970,15:389
  • 7Fu Y,Batchelor A W,Wang Y et al.Wear[J],1998,217(1):132
  • 8Xu Guizhen,Zhou Zhongrong,Liu Jiajun.Wear[J],1999,224(2):211
  • 9Zhu M H,Zhou Z R.Surface and Coatings Technology[J],2001,141(2-3):240
  • 10JiangBin(蒋斌) XuBinshi(徐滨士) DongShiyu(董世运)etal.Tribology(摩擦学学报),2002,22(4):185-185.

引证文献5

二级引证文献49

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部