摘要
高炉锰铁中的硅来自焦炭灰分和部分锰渣中的SiO2。硅还原过程为SiO2-SiO-[Si]。使用高Mn低SiO2的进口富锰矿,因其焦比低渣量少,造成锰铁[Si]低,因此它不仅提高锰含量而且提高货物等级。
Silicon resource comes from coke ash and parts of SiO2 in manganese slag. Silicon reducts to SiO2 - SiO - [ Si] . Import manganese - rich ore, which is rich in manganese and poor in SiO2, leads to coke rate lower and slag less. This is why silicon low in ferromanganese. It raises not only manganese grade but also its level.
出处
《铁合金》
北大核心
2005年第4期1-3,共3页
Ferro-alloys
关键词
高炉
富矿
锰铁
研究
blast furnace, rich ore, ferromanganese, research