摘要
锌基合金(ZA22,ZA27)可以挤压和轧制成形,但挤压成形塑性偏低。通过固溶后自然时效处理,可有效地提高合金的综合力学性能;挤压后直接人工时效,可有效地提高合金的塑性。
Zinc-based alloys(ZA22,ZA27) may be formed by rolling and extrusion but with lower plasticity after extruding.The results indicate that natural ageing after solution heat-treatment leads to the effective increasement of the comprehensive mechnical properties.Moreover,after extruding the alloys can improve their plasticity if artificial ageing is processed.
出处
《热加工工艺》
CSCD
北大核心
1996年第2期26-28,共3页
Hot Working Technology