1Yang X H, Zhang Y M, Han J C. High speed lapping of SiC ceramic material with fixed abrasive [ J]. High Performance Ceramics IV, 2007, 336-338 : 1458-1460.
2David, Edwards F, Paul Hed P. Optical element manufacturing [J]. Applied Optics, 1987, 26: 23-28.
3Lin T R, Su C R. Experimental study of lapping and electro-polishing of tungsten carbides [ J ]. International journal of advanced manufactur- ing technology, 2008, 36:715-723.
4Zheng X F, Yuan J L, Wen D H. Parameters optimization on the lap- ping process of 9Cr18 with Taguchi method [ J ]. Advances in Grinding and Abrasive Technology XIV, 2008, 359-360 : 158-161.
5Chang Y P, Hashimura M, Dornfeld D A. An investigation of material removal mechanisms in lapping with grain size transition [ J ]. Journal of Manufacturing Science and Engineering- transactions of the ASME, 2000, 122(3) : 413-419.
6Deshpande L S, Raman S, Sunanta O. Observations in the flat lapping of stainless steel and bronze [ J ]. Wear, 2008,265 ( 1/2 ) : 105-116.