四川乐山大佛风化的初步探讨 被引量:26

A study on weathering processes of Leshan Grand Buddha,Sichuan,China
下载PDF
导出
摘要 四川乐山大佛石刻是我国重要的'世界文化与自然遗产'之一,石刻表面毁损非常严重.本文通过(1)检测石刻所在地区粉砂岩的样品成分(XRFS)获悉,SiO2含量高达84%;(2)安装微侵蚀测量装置(MEM)直接测得粉砂岩的表面侵蚀速率大约为0.216~0.305mm/a;结合(3)粉砂岩表面的相对硬度测试比较等途径,对石刻毁损的表面过程机制进行了初步的综合分析.结果表明,由于粉砂岩结构松散,经水浸后表面硬度急剧下降,而且当地的水、气等条件适宜于生物繁衍等特点,石刻风化毁损的原因主要在于水、生物等环境因素对粉砂岩胶结物有强烈的破坏作用. Leshan Grand Buddha is one of the most important heritage resources of the World Heritage of Culture and Nature in China, which is located in Lingyun Mountains at Leshan, Sichuan province, China. The surface weathering problem of the carved stone is very serious, and how to protect it from the bad weathering is a difficult task. Therefore, this paper studies on the surface weathering problems of the siltstone in Lingyun Mountains, where Leshan Grand Buddha is located, in order to get more deterioration information about the carved stones. The test results of the siltstone samples with the X-ray Fluorescence Spectrometry (XRFS) indicated that the SiO2 is the main component and its quality percentage is up to 84 %, the next parts are Al2O3 of 7.5 % and Fe2O3 of 1.7 %, etc. In addition, the siltstone includes a great deal of quartz powder, most of its diameter is around 0. 250mm, and the other is the mauve cementation. In order to measure the erosion rates of the siltstone, we installed four suits of microerosion meter (MEM) instruments based on the principle of screwing measurement. The results indicated that the erosion thickness is mostly close 0. 216-0. 303ram of the year. We also investigated the environmental factors besides the experiment and found that water and biological intrusions are two important factors affecting the erosion rates. At the locale, we also tested the rigidity of the siltstone surfaces too with grout rebound instrument (ZC5 Model), which proved that siltstone weathering is faster than that of limestone because of the very low rigidity. The surface rigidity of siltstone will reduce quickly and become soft once it touches water, so the siltstone surface is easy to be destroyed by environmental factors. Therefore we can conclude that the Leshan Grand Buddha will go on weathering because the siltstone rocks has loose structure, and siltstone surface can be ruined easily. The good natural environment such as water vapor from the river, complex components of the siltstone cementation conditions is favorable for the microorganism and plants to grow. Therefore, water and bio-environment are important external factors accelerating the heritage surface deterioration and the fundamental internal factor is the unstable structure of the quartz grain and cementation system.
出处 《地理研究》 CSCD 北大核心 2005年第6期928-934,共7页 Geographical Research
基金 国家自然科学基金资助项目(40271017)
关键词 乐山大佛 石刻遗产 粉砂岩 侵蚀速率 Leshan Grand Buddha stone heritage siltstone erosion rates
  • 相关文献

参考文献20

  • 1Monforti F, Bellasio R, Bianconi R, et al. An evaluation of particle deposition fluxes to cultural heritage sites in Florence, Italy. Science of the Total Environment, 2004, 334-335(1): 61~72.
  • 2Satake K, Inoue T, Kasasaku K, et al. Monitoring of nitrogen compounds on Yakushima Island, a world natural heritage site. Environmental Pollution, 1998, 102(1): 107~113.
  • 3Pitzurra L, Moroni B, Nocentini A, et al. Microbial growth and air pollution in carbonate rock weathering. International Biodeterioration and Biodegradation, 2003, 52(2): 63~68.
  • 4Walderhaug O. Chemical weathering at rock art sites in Western Norway: which mechanisms are active and how can they be retarded? Journal of Archaeological Science, 1998, 25(8): 789~800.
  • 5Delalieux F, Cardell C, Todorov V, et al. Environmental conditions controlling the chemical weathering of the Madara Horseman monument, NE Bulgaria. Journal of Cultural Heritage, 2001, 2(1): 43~54.
  • 6屈建军,张伟民,王远萍,贺大良,戴枫年,文子祥,王家澄.敦煌莫高窟古代生土建筑物风蚀机理与防护对策的研究[J].地理研究,1994,13(4):98-104. 被引量:9
  • 7Petuskey W T, Richardson D A, Dolske D A. Aspects of the deterioration of sandstone masonry in Anasazi dwelling ruins at Mesa Verde National Park, Colorado, USA. The Science of the Total Environment, 1995, 167(1-3): 145~159.
  • 8Pope G A, Meierding T C, Paradise T R. Geomorphology's role in the study of weathering of cultural stone. Geomorphology, 2002, 47(2-4): 211~225.
  • 9张捷,李升峰,陈舒泛,杨天麒.南京梁代石刻微侵蚀的研究[J].地理学报,1994,49(5):418-428. 被引量:8
  • 10曹建华,王福星,黄俊发,黄基富,王晶.桂林地区石灰岩表面生物岩溶溶蚀作用研究[J].中国岩溶,1993,12(1):11-22. 被引量:27

二级参考文献29

共引文献122

同被引文献381

引证文献26

二级引证文献95

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部