瓦楞纸箱开孔对耐压强度的影响 被引量:8

The Effects of Holing Corrugated Fiber Box on Pressure-resisting Strength
下载PDF
导出
摘要 通过试验,分析开孔对瓦楞纸箱耐压强度的影响。指出开孔位置与侧板中线的距离小于长度的八分之三为适宜,扁丝接合的瓦楞纸箱与其它方式接合的瓦楞纸箱相比,其耐压强度最低。 Based on various experiments, This paper provides an analysis of the effects of holing corrugated fiber box on pressure-resisting strength, Pointing out that the desirable distance between the holding point and the middle line of the side board should be less than the three eighthes of the whole lengtl and that the pressure-resisting strength of the flat-nail jointed corrugated fiber box is the lowest, in comparision with that of other kinds of the corrugated fiber boxes.
机构地区 株洲工学院
出处 《包装工程》 CAS CSCD 1996年第3期22-24,共3页 Packaging Engineering
关键词 瓦楞纸箱 耐压强度 接合 开孔 包装材料 Corrugated fiber box Pressure-resisting strength Joint