摘要 回顾和分析了管线钢DWTT方法的建立过程、应用情况以及在高强度、高韧性、大壁厚管线钢中存在的DWTT异常断口问题。在综述目前该问题研究现状的基础上,通过研究和分析,提出了对DWTT异常断口的基本看法和处理方法。 The establishment and application of the DWTT method are reviewed. The abnormal fracture during DWTT of high strength, high toughess pipeline steel for thick wall pipes is also described. Based on the study the reason and countermeasures of abnormal fracture during DWTT are put forward.
出处 《钢铁研究学报》 CAS CSCD 北大核心 2005年第6期1-5,共5页 Journal of Iron and Steel Research
基金 中国石油天然气集团公司技术开发项目(04B41102)
关键词 管线钢 DWTT异常断口 压制缺口 评判方法 pipeline steel DWTT abnormal lracture pressed notch evaluation methods
  • 相关文献

参考文献17

  • 1Eiber R J.Correlation of Full-Scale Tests with Laboratory Test [A].Proceeding of 2nd Symposium on Line Pipe Re-search [C].Texas,Dallas: Pipeline Research Committee ofAGA L30000,1965.83-118.
  • 2Fearnehough G D.Fracture Propagation Control in Gas Pipe-line [A].Crack Propagation in Pipelines [C].England,New-castle Upon Tyne: The Institution of Gas Engineers,1974.
  • 3Eiber R J.Fracture Propagation [A].Proceeding of 2nd Sym-posium on Line Pipe Research [C].Texas,Dallas: Pipeline Research Committee of AGA L30000,1965.21-42.
  • 4API RP 5L3,API Recommended Practice for Conducting Drop Weight Tear Test on Line Pipe,3rd Edition [S].
  • 5JFE钢铁公司.与JFE关于DWTT异常断口评判的内部交流资料[R].,2004..
  • 6API Specification 5L,Specification for Line Pipe,Forty-Second Edition [S].
  • 7ISO 3183-3,Petroleum and Natural Gas Industries-Steel Pipefor Pipelines-Technical Delivery Conditions-Part 3: Pipes of Requirement Class C,First Edition [S].
  • 8Q/SYXQ15-2003.西气东输管道工程直缝埋弧焊管技术条件[S].[S].,..
  • 9Q/SYJS0018-2003.陕京二线管道直缝埋弧焊钢管技术条件[S].[S].,..
  • 10A-SS101,High Strength Steel Line Pipe [S].

二级参考文献11

  • 1.GB 2038-91.金属材料延性断裂韧度JIC试验方法[S].,..
  • 2中国石油天然气(集团)公司石油管材研究所.西气东输管线X70试验卷板试验评价报告[R].西安: 中国石油天然气(集团)公司石油管材研究所,2000..
  • 3.GB 4161-84.金属材料平面应变断裂韧性KIC试验方法[S].,1984..
  • 4Guo W, Dong H, Lu M, et al. The Coupled Effects of Thickness and Delamination on Cracking Resistance of X70 Pipeline Steel[J]. International Journal of Pressure Vessels and Piping, 2002,79(6) :403-412.
  • 5ASTM E399-83, Standard Test Method for Plane-Strain Fracture Toughness of Metallic Materials [S].
  • 6Hertzberg R W. Deformation and Fracture Mechanics of Engineering Materials[M].New York: John Wiley & Sons, 1976,.
  • 7ASTM E813-81, Metallic Materials-Standard Test Method for Jlc, a Measure of Ductile Fracture Toughness [S].
  • 8中国石油天然气(集团)公司石油管材研究所.西气东输管线X70试验卷板试验评价报告[R].西安:中国石油天然气(集团)公司石油管材研究所,2000..
  • 9GB4161-84.金属材料平面应变断裂韧性Klc试验方法[S].[S].,..
  • 10GB2038-91.金属材料延性断裂韧度Jlc试验方法[S].[S].,..

共引文献14

同被引文献238

引证文献38

二级引证文献143

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部