摘要 在常规PET生产中加入适当的第三单体和第四单体可制备低熔点聚酯。以精对苯二甲酸(PTA)和乙二醇(EG)为原料,加入适当的间苯二甲酸(或己二酸)、1,4-丁二醇(或6-己二醇),聚乙二醇的质量分数(相对二元羧酸)为5%~8%,采用质量分数为0.005%~0.008%钛系催化剂,生产的低熔点聚酯熔点为110~120℃,且热稳定性好。 A low-melting point PET can be produced by adding the proper third and forth monomers during regular PET production. The low-melting point PET with the melting point in the range of 110 - 120℃and good thermal stability can be produced from purified terephthalic acid and ethylene glycol by adding proper amount of isophthalic acid or adipic acid and 1,4-butanediol or 1,6-hexamethylene glycol, 5% -8% polyethylene glycol based on dicarboxylic acid and 0. 005% -0. 008% Ti-containing catalysts by mass fraction.
作者 陆宏良
出处 《合成纤维工业》 CAS CSCD 北大核心 2005年第6期40-41,共2页 China Synthetic Fiber Industry
关键词 聚对苯二甲酸乙二酯 低熔点聚酯 共聚 力学性能 催化剂 制备 polyethylene terephthalate low-melting point polyester copolymerization mechanical property catalyst preparation
  • 相关文献

同被引文献60

引证文献8

二级引证文献32

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部