A series of supported molybdenum phosphide catalysts were prepared by impregnation method. XRD, TG-DTG, XPS and BET were used to study the phase, compositions and surface areas of the prepared catalysts. A model reactant containing thiophene, pyridine and cyclohexene was used for the measurements of catalytic activities. The effect of reduction temperature on catalytic activities was investigated. The analysis results by XRD and BET are very different when the reduction temperature is changed from 400 to 900 ℃. MoP/γ-Al2O3 catalysts and CoMoP/γ-Al2O3 catalysts prepared at the reduction temperature of 500 ℃ are the most active ones.
A series of supported molybdenum phosphide catalysts were prepared by impregnation method. XRD, TG-DTG, XPS and BET were used to study the phase, compositions and surface areas of the prepared catalysts. A model reactant containing thiophene, pyridine and cyclohexene was used for the measurements of catalytic activities. The effect of reduction temperature on catalytic activities was investigated. The analysis results by XRD and BET are very different when the reduction temperature is changed from 400 to 900 ℃. MoP/γ-Al2O3 catalysts and CoMoP/γ-Al2O3 catalysts prepared at the reduction temperature of 500 ℃ are the most active ones.