摘要
采用显微硬度计、电子拉伸试验机、光学显微镜和TEM等,通过与Cu-0.1%Ag合金对比,分析了Cu-0.1%Ag-0.06%Ce合金和Cu-0.1%Ag-0.1%Cr合金的抗软化性能、合金元素的作用及组织形貌特征。结果表明:Cu-0.1%Ag合金中分别加入铬和稀土铈后,综合性能明显提高,软化温度分别提高了110和35℃,稀土化合物以小球状分布在晶体内,细化晶粒,提高硬度(强度)和抗软化性能。
Resistance to softening, the effects of alloy elements and microstructures of Cu-0.1% Ag-0.06% Ce and Cu-0.1% Ag-0. 1% Cr alloys were analyzed and compared with Cu-0.1% Ag ahoy, by using hardometer, electronic tensile testing machine, optical microscope and TEM, etc. The results indicate that the comprehensive properties of Cu-0.1% Ag alloy remarkably are improved after adding traces of Cr and rare earth Ce elements respectively. Softening temperatures rise by 110 and 35℃ respectively and the rare earth compounds of small ball shapes can refine grain sizes and improve strength or hardness and resistance to softening property.
出处
《稀有金属》
EI
CAS
CSCD
北大核心
2006年第1期39-42,共4页
Chinese Journal of Rare Metals
基金
国家高技术研究发展计划资助项目(2002AA331110)
关键词
铜合金
接触线
时效
铜银合金
copper alloy
contact wires
aging
Cu-Ag alloy